Background: The Critical Challenge
A monorail crane operator was facing severe equipment safety hazards. The friction blocks previously in use exhibited extreme brittleness under actual working conditions, leading to complete structural fragmentation (shattering) during high-speed operation or emergency braking.
*Consequences: This led to brake failure and costly production downtime. Furthermore, debris from the shattered blocks frequently became lodged in the rail system, causing secondary mechanical damage to surrounding components.
Solving the Warping Issue on SIBRE SHI202 (520x195x20mm) Brake Pads
(1) On-Site Engagement: Pinpointing Three Critical Pain Points
(2) Targeted Innovation: A Systematic Technical Response
(3) Proven Results: Recognition and Volume Orders